Originally Posted by
Roger Koh
>>> A lot of the cracks have smoothed out, some cracks still look rough with a smooth texture. This might be the best I can do. Will do one more application to see if it changes (the rougher areas) If not, it will be the best I can do.
Severe cracks will require repairs from a combination of Bond-3D + Stucco-90 + Anilne-76 – mixed up, fill-up, and level up with a plastic card and wipe off surface excess. Repeat each time as the water contents evaporates and the filling shrinks. When all smooth out (sanding with 1500/2000 grit), Adhesor-73 application will seal and balance out the absorbency rate ready for Aniline-76.